Copper phosphate glass with composition of 20Li2O-30CuO-50P2O5(in mol%) was prepared with an improved method. The electrical properties were measured after the samples were heat-treated for 1,2,4,8 and 12 hours, respectively.
英
美
释义
本文采用一种新的成形工艺制备20Li2O-30CuO-50P2O5(摩尔比)玻璃,并在玻璃转变温度之上对样品进行了不同时间的热处理后测试了其电性能。