HAZ cracking was associated with prior particle boundaries and was influenced by HIP parameters.The electron microprobe, SEM, and STEM were used to characterize the cracking.
英
美
释义
文章摘要: The weld cracking susceptibility of the HAZ of HIPed stainless steels was evaluated using both the Varestraint Test and Gleeble hot ductility test.